the printer begins very well but after 40%-50% of printing the part unstuck from the heated bed. I use 60 degrees in heated bed, Build Plate Adhesion - Brim. Any suggestions?
top of page
To see this working, head to your live site.
2 Comments
bottom of page
Reducing the Z-offset to get better first layer adhesion should help.
Are you printing with PLA? The recommended temperature for PLA on the heated bed is 45C. It's possible that 60 is too hot.